SANTA CLARA, Calif. – July 9, 2020 – Materials enhancements in two new electrically conductive elastomers from Laird R and F Products eliminate the risk of galvanic corrosion and damage from fuel, oils and deicing fluids in military and aerospace applications. Laird can manufacture the new elastomers using highly resilient fluorosilicone and either nickel aluminum or passivated silver aluminum fillers, offering reliable mechanical, environmental and electromagnetic shielding capabilities.
“Our new electrically conductive elastomers provide reliable environmental sealing and electromagnetic interference shielding for military equipment in the harshest environments,” said Rick Johnson, aerospace and defense director at Laird R&F Products. “These two new products expand our line of elastomers and help design engineers protect military electronics amid exposure to saltwater, missile fuel and more.”
EcE 130 is an electrically conductive fluorosilicone elastomer featuring conductive passivated silver aluminum filler. The silver aluminum material offers high surface conductivity, eliminating energy leakage and reducing signal interference. The added passivation helps the elastomer resist damaging galvanic corrosion.
EcE 135 is an electrically conductive fluorosilicone elastomer featuring nickel aluminum filler. The nickel’s inert properties are compatible with all other metals, offering better corrosion resistance than other filler materials.
“Laird regularly explores new materials to help our military and aerospace customers respond to their complex and evolving challenges,” Johnson said. “The nickel and passivated silver aluminum materials in these new elastomers offer military and aerospace design engineers additional environmental and EMI sealing capabilities, helping them improve the functionality and reliability of electronic systems across a wider range of applications.”
Laird R&F Products offers end-to-end elastomer solutions for the military and aerospace industries with a product line that includes 40 different compounds and silicone, fluorosilicone, and EDPM elastomers.
To learn how Laird R&F Products devised a novel seal solution to protect vital equipment on a military fighter jet, click here.
About Laird
Laird Performance Materials, a portfolio company of Advent International, enables high-performance electronics. We create advanced protection solutions for electronic components and systems. World-leading technology brands rely on us for improved protection, higher performance and reliability, custom structural designs and faster time-to-market. We solve design issues through innovative products such as EMI suppression or absorption materials, thermal interface materials, structural and precision metals, magnetic ceramic products, and multi-functional solutions. This latter product family solves multiple EMI, thermal, and structural design issues simultaneously using a single process solution. Visit https://www.laird.com.